Category

TPU Film for TPU Flooring, Wear resistance, flame retardant, Anti-UV

  • BASIC PHYSICAL PERFORMANCE

Specifications:
Thickness: 0.05-2.0mm (can be customized)
Width: 10-1500mm (can be customized)
Color: transparent, foggy (any colors can be customized)

 

Advantages
Polyester TPU film has better heat resistance and chemical solvent resistance, good air tightness AND easy to process, widely used to replace PVC film for various purposes.
Processing is simple and convenient: TPU film is easier to process than PVC film by means of high frequency, hot pressing and other processing methods, it is better than PVC film after appropriate adjustment of hot pressing time, temperature and pressure.
Acid and alkali oil resistance: polyester TPU film is a strong polar polymer material, and non-polar mineral oil affinity is very small, almost no erosion in fuel oil and machinery oil.
Aging and oxidation resistance: polyester film has better physical properties, such as tear strength, tensile strength, elongation, etc.Therefore, its aging resistance and oxidation resistance is also good.Better air tightness: suitable for air bag cushion, inflatable products and blowing toys.
It can be widely used to replace various uses of PVC films.

 

TPU Films Flame Retardant Testing:

Report No: 202405141001
Test Dept: XIN GEN R&D Dept.                                                       
Test Item: Vertical Combustion
Test Standard: GB/T 8624.GB/T 8626
Test Location: Constant Temperature and Humidity Laboratory of Technology Center Processing Laboratory
Sample Size: 305 mm x 76 mm x 0.2mm
Test Result: See following table
Test Environment: 23℃/50%RH
Test Date: 2024/5/14



Sample No.

XG1185-02 (T22120801)

Warp And Weft Of The Sample

CD

CD

CD

MD

MD

MD

Whether it ignites or not

YES

YES

YES

YES

YES

YES

Whether it reaches 150mm

NO

NO

NO

NO

NO

NO

Whether the filter paper is ignited

NO

NO

NO

NO

NO

NO

Conclusion

Can reach B1 B Grade

Note: According to GB/T8624, B1B level shall be tested according to the ignition time 30S method in GB/T8626



BASIC PHYSICAL PERFORMANCE:

TEST ITEM

TEST METHOD

UNIT

TEST VALUE

Hardness

ASTM D2240

Shore A

85

Thickness

ASTM D3767

mm

0.3

Specific Gravity

ASTM D792

g/cm³

1.2

Colour

Visual Inspection

/

FOGGY

Tensile Strength

ASTM D412/Die C

MPa

CD59.35    MD51.76

100%MOD

ASTM D412/Die C

MPa

CD6.25    MD6.18

300%MOD

ASTM D412/Die C

MPa

CD12.05    MD12.02

Elongation at Break

ASTM D412/Die C

%

CD704    MD653

Tear Strengthnotes1

ASTM D624

KN/m

CD93.2    MD106.2