Air Medical Mattress/Cushion
Material-Fabric | Material-TPU | TPU Type | TOTAL Weight | Total Thickness | Color | Surface | Application |
70D Nylon | 0.08mm | Ether/Ester | 170gsm | 0.18mm | Blue,White,Black,Grey,can be customized | Glossy/Matte | ![]() |
70D Nylon | 0.09mm | Ether/Ester | 180gsm | 0.19mm | Glossy/Matte | ||
70D Nylon | 0.10mm | Ether/Ester | 210gsm | 0.20mm | Glossy/Matte | ||
210D Nylon | 0.10mm | Ether/Ester | 230gsm | 0.25mm | Glossy/Matte | ||
210D Nylon | 0.15mm | Ether/Ester | 300gsm | 0.30mm | Glossy/Matte | ||
210D Nylon | 0.20mm | Ether/Ester | 380gsm | 0.35mm | Glossy/Matte | ||
210D Nylon | 0.34mm | Ether/Ester | 520gsm | 0.45mm | Glossy/Matte |
Air Medical Mattress/Cushion
Material-Fabric | Material-TPU | TPU Type | TOTAL Weight | Total Thickness | Color | Surface | Application |
70D Nylon | 0.08mm | Ether/Ester | 170gsm | 0.18mm | Blue,White,Black,Grey,can be customized | Glossy/Matte | ![]() |
70D Nylon | 0.09mm | Ether/Ester | 180gsm | 0.19mm | Glossy/Matte | ||
70D Nylon | 0.10mm | Ether/Ester | 210gsm | 0.20mm | Glossy/Matte | ||
210D Nylon | 0.10mm | Ether/Ester | 230gsm | 0.25mm | Glossy/Matte | ||
210D Nylon | 0.15mm | Ether/Ester | 300gsm | 0.30mm | Glossy/Matte | ||
210D Nylon | 0.20mm | Ether/Ester | 380gsm | 0.35mm | Glossy/Matte | ||
210D Nylon | 0.34mm | Ether/Ester | 520gsm | 0.45mm | Glossy/Matte |
Material-Fabric | Material-TPU | TPU Type | TOTAL Weight | Total Thickness | Color | Surface | Application |
70D Nylon | 0.10mm | Ether/Ester | 210gsm | 0.20mm | Can be customized | Glossy/Matte | ![]() |
210D Nylon | 0.15mm | Ether/Ester | 300gsm | 0.30mm | Glossy/Matte | ||
Non Woven | 0.15mm | Ether/Ester | 300gsm | 0.30mm | White |
Glossy/Matte |
Material-Fabric | Material-TPU | TPU Type | TOTAL Weight | Total Thickness | Color | Surface | Application |
"95-100g DOUBLE KNAP KNIT Nylon" | 0.15mm | Ether/Ester | 260gsm | 0.30mm | Grey, Black, Blue, can be customized | Glossy/Matte | ![]() |
"95-100g UBL TRICOT KNIT 100% 40 DENIER NYLON" | 0.15mm | Ether/Ester | 260gsm | 0.30mm | Glossy/Matte |
Descriptions
1. Test items: Tensile,Tearing and Adhesion Strength, Weight,Thickness,etc.
2. Tested Condition: Temperature:25℃; Humidity:55%
3.Testing Machine: Tensile Testing Machine
4.Test Result: (based on average)
Product Name | 210T Nylon TPU Materail | |||||
Spec | 0.20/1390mm | |||||
No. | Test Items | Uint | Test Result | Limit | Test Method | |
1 | Total Thickness | mm | 0.21 | 0.20±0.02 | DIN EN ISO 2286-2 | |
2 | Total Weight | g/m2 | 215 | ˉ | ||
3 | Width | mm | 1390 | 1390±5 | ||
4 | Hardness | Shore A | 85 | 85±2 | ASTM D2240 | |
5 | fabric | Weight | g/m2 | 63 | 60-65 | ˉ |
Yarn | T | 70D*107T*86T | ˉ | |||
6 | Tensile Strength | Warp | N/5cm | 740 | ≥500 | DIN 53354 |
Weft | 452.3 | ≥400 | ||||
7 | Elongation | Warp | % | 35.2 | ≥30 | DIN 53354 |
Weft | 34.1 | ≥30 | ||||
8 | Tear Strength | Warp | N | 12 | ≥8 | DIN 53329 |
Weft | 15 | ≥8 | ||||
9 | Adhesion Strength | Face | N/3cm | 35 | ≥30 | Match JIS |
10 | Color Fastness To Washing | / | Grade 4-5 | ≥Grade 4 | ISO 105-C06:2010 | |
11 | Result | Qualified |
"NOTE:
1.The test data in the report is only for samples, and for reference only;
2. the test data,without permission,shall not arbitrarily modify. If need to modify, the modified data must have the signature(Seal) of the experimenter."
Descriptions
1. Test items: Tensile,Tearing and Adhesion Strength, Weight,Thickness,etc.
2. Tested Condition: Temperature:25℃; Humidity:55%
3.Testing Machine: Tensile Testing Machine
4.Test Result: (based on average)
Product Name | 210D Nylon TPU Material | |||||
Spec | 0.25 / 1480mm | |||||
No. | Test Items | Uint | Test Result | Limit | Test Method | |
1 | Total Thickness | mm | 0.25 | 0.25±0.02 | DIN EN ISO 2286-2 | |
2 | Total Weight | g/m2 | - | - | ||
3 | Width | mm | 1480 | 1480±5 | ||
4 | Hardness | Shore A | 85 | 85±2 | ASTM D2240 | |
5 | Tensile Strength | Warp | N/5cm | 831 | ≥500 | DIN 53354 |
Weft | 620 | ≥500 | ||||
6 | Elongation | Warp | % | 50 | ≥30 | DIN 53354 |
Weft | 38 | ≥30 | ||||
7 | Tear Strength | Warp | N | 25.6 | ≥8 | DIN 53363 |
Weft | 22 | ≥8 | ||||
8 | Adhesion Strength | Face | N/3cm | 38 | ≥30 | DIN 53357 |
9 | Color Fastness To Washing | / | Grade 4-5 | ≥Grade 4 | ISO 105-C06:2010 | |
10 | Result | Qualified |
"NOTE:
Descriptions
1. Test items: Tensile,Tearing and Adhesion Strength, Weight,Thickness,etc.
2. Tested Condition: Temperature:25℃; Humidity:55%
3.Testing Machine: Tensile Testing Machine
4.Test Result: (based on average)
Product Name | 420D Nylon TPU Material | |||||
Spec | 0.40 / 1470mm | |||||
No. | Test Items | Uint | Test Result | Limit | Test Method | |
1 | Total Thickness | mm | 0.39 | 0.40±0.02 | DIN EN ISO 2286-2 | |
2 | Total Weight | g/m2 | 360 | - | ||
3 | Width | mm | 1470 | 1470±5 | ||
4 | Hardness | Shore A | 85 | 85±2 | GB/T 2411 | |
5 | Tensile Strength | Warp | N/5cm | 1352 | ≥900 | HG/T 2580 |
Weft | 620 | ≥500 | ||||
6 | Elongation | Warp | % | 43 | ≥30 | HG/T 2580 |
Weft | 53 | ≥30 | ||||
7 | Tear Strength | Warp | N | 33 | ≥10 | HG/T 2581 |
Weft | 25 | ≥8 | ||||
8 | Adhesion Strength | Face | N/3cm | 52 | ≥50 | EN ISO 2411 |
9 | Result | Qualified |
"NOTE:
1.The test data in the report is only for samples, and for reference only;
2. the test data,without permission,shall not arbitrarily modify. If need to modify, the modified data must have the signature(Seal) of the experimenter."